The stress corrosion resistance of ZA-27 TiO2 metal matrix composites MMC's in high temperature acidic media has been evaluated using an autoclave. The liquid melt metallurgy technique using vortex method was used to fabricate MMC's. TiO2 particulates of 50-80 µm in size are added to the matrix. ZA-27 containing 2, 4, 6 weight percentage of TiO2 are prepared.
Stress corrosion tests were conducted by weight loss method for different exposure time, normality and temperature of the acidic medium. The corrosion rates of composites were lower to that of matrix ZA-27 alloy under all conditions.
by K. Vinutha | P. V. Krupakara | H. R. Radha "Stress Corrosion Studies of Titanium Dioxide Particulate Reinforced ZA-27 Metal Matrix Composites"
Published in International Journal of Trend in Scientific Research and Development (ijtsrd), ISSN: 2456-6470, Volume-2 | Issue-6 , October 2018,
URL: http://www.ijtsrd.com/papers/ijtsrd18739.pdf
Direct Link: http://www.ijtsrd.com/chemistry/physical-chemistry/18739/stress-corrosion-studies-of-titanium-dioxide-particulate-reinforced-za-27-metal-matrix-composites/k-vinutha
call for paper papers conference, international journal of management, research papers


No comments:
Post a Comment